General Information
Ovako 146S is an ingot cast case hardening steel with good dimension stability and high toughness. The chemical composition is well controlled to give the steel a controlled hardenability towards the high end of the EN 10084:1998 range for 16NiCrS4. It has reduced silicon content for reduced propensity for internal oxidation during carburizing. Regulated sulphur content ensures good machinability properties.
For additional Heat Treatment Data, please visit the Heat Treatment Guide
Similar designations
SS 2511, 16NCD5 (AFNOR), 637 A 16 (BS)
Other properties (typical values)
Youngs module (GPa) | Poisson´s ratio (-) | Shear module (GPa) | Density (kg/m3) |
210 |
0.3 |
80 |
7800 |
Average CTE 20-300°C (µm/m°K) | Specific heat capacity 50/100°C (J/kg°K) | Thermal conductivity Ambient temperature (W/m°K) | Electrical resistivityAmbient temperature (µΩm) |
12 |
460 - 480 |
40 - 45 |
0.20 - 0.25 |
Disclaimer
The information in this document is for illustrative purposes only. The data and examples are only general recommendations and not a warranty or a guarantee. The suitability of a product for a specific application can be confirmed only by Ovako once given the actual conditions.The purchaser of an Ovako product has the responsibility to ascertain and control the applicability of the products before using them. Continuous development may necessitate changes in technical data without notice. This document is only valid for Ovako material. Other material, covering the same international specifications, does not necessarily comply with the properties presented in this document.